Study on severe deterioration of outer layer and edges of concrete due to H2S exposure. Importance of surface prep and Quadex Aluminaliner application for 5000 psi required strength. Successful results after Raven 405 application and 5 years of inspection.
E N D
Effects of H2S on Concrete Case Study Cary N.C. Outer layer of concrete is severely deteriated Edges is badly deteriorated
Surface prep is critical Sound Concrete Is Required 5000 psi at 5 gpm 0 degree rotating nozzle
After Build Back of ½” to 1” Quadex Aluminaliner
After application of 120 Mils of Raven 405
After 5 yrs Very Severe H2s Inspection revealed not one failed area