An Image/Link below is provided (as is) to download presentation Download Policy: Content on the Website is provided to you AS IS for your information and personal use and may not be sold / licensed / shared on other websites without getting consent from its author. Content is provided to you AS IS for your information and personal use only. Download presentation by click this link. While downloading, if for some reason you are not able to download a presentation, the publisher may have deleted the file from their server. During download, if you can't get a presentation, the file might be deleted by the publisher.

E N D

Presentation Transcript


  1. Babbitt Metalizing Wire Babbitt Metalizing Wire For Thermal Spray Process Babbitt metalizing wire is an additional alloy of tin. Babbitt has been applied to varied similar white metals comprised of tin, copper, and metals. The lead will typically be supplemental in situ of the tin. Metalizing wires widely used in the thermal spray coating process to provide a thick coating layer to prevent oxidation. Babbitt alloys provide corrosion resistance, excellent wetting, low wear and friction resistance, and unit of activity proverbial for its hard/soft composition. whereas the tin and lead unit of activity soft, the copper and metal kind exhausting crystals throughout the structure. The carrying of the softer metal permits for higher absorption of the lubricator jointly as any foreign particles. Babbitt metal is used as a result of the liner for bearing shells of robust, steel, and bronze. The metalizing wire lining stops friction and wears that's common once a lubricator isn't ready to stop the bearing’s moving parts from the attachment on. The Babbitt thus extends the amount of your time of the bearing. Users of alloy bars soften the metal in iron kettles from that they are aiming to ladle or pump the liquified alloy. The bearing shell or backing is pre-coated with tin for tin-based bearings or with lead/tin for lead-based bearings. Whereas the coating continues to be liquified, the alloy is solid onto the backing and allowed to solidify from the bond inward. This prevents contraction cavities at the bond and restricts the expansion of intermetallic compounds at the interface between the

  2. bearing shell and jointly the Babbitt. the liner is then machined to a mirror-bright end and like thickness. Babbitt wire can even be sprayed onto the bearing shell with the use of a flame spray gun, metalizing gun, arc spray gun, and Babbitt wire. Babbitt Metalizing Wire Chemical Composition Tin Base Chemical Composition(%) Alloy Number(Grade) 1 2 3 11 Tin 90.0-92.0 88.0-90.0 83.0-85.0 86.0-89.0 Antimony 4.0-5.0 7.0-8.0 7.5-8.5 6.0-7.5 Lead 0.35 0.35 0.35 0.5 Copper 4.0-5.0 3.0-4.0 7.5-8.5 5.0-6.5 Iron 0.08 0.08 0.08 0.08 Arsenic 0.1 0.1 0.1 0.1 Bismuth 0.08 0.08 0.08 0.08 Zinc 0.005 0.005 0.005 0.005 Aluminum 0.005 0.005 0.005 0.005 Cadmium Total Named Elements, Min. 0.05 0.05 0.05 0.05 99.8 99.8 99.8 99.8 Lead Base Alloy Number(Grade) 7 9.3-10.7 14.0-16.0 14.0-16.0 9.5-10.5 Remainder Remainder Remainder 0.5 0.5 0.1 0.1 0.30-0.60 0.30-0.60 0.25 0.1 0.1 0.005 0.005 0.005 0.005 Chemical Composition(%) 8 4.5-5.5 13 5.5-6.5 15 86.0-89.0 6.0-7.5 Remainder 0.5 0.1 0.8-1.4 0.1 0.005 0.005 Tin Antimony Lead Copper Iron Arsenic Bismuth Zinc Aluminum 0.5 0.1 0.1 0.005 0.005

  3. Cadmium Total Elements, Min. 0.05 0.05 0.05 0.05 Named Babbitt metalizing Wire #2 Babbitt metalizing wire #2 consists of tin, Sb, and copper. this can be such as ASTM B-23 #2. This alloy incorporates a melting temperature of 240-355° C (466-669° F). Babbitt metalizing wire #2 may be a high tin Babbitt, which is typically used for top operative temperatures and high unit load. These materials show superb corrosion resistance, simple bonding, and fewer tendencies for segregation and fastening. They are preferred to be used beneath steady load conditions in steam and gas turbines, electrical motors, blowers, and pumps. Babbitt Metalizing Wire #7 Babbitt metalizing wire #7 consists of lead, antimony, tin, and arsenic. this can be such as ASTM B-23 #7. This alloy incorporates a melting temperature of 240-268° C (466- 514° F). Babbitt metalizing wire #7 is usually used for sleeve bearings operative at moderate hundreds and speeds like bearings for blowers, pumps, electric motors, and machine tools. Co –Babbitt Metalizing Wire Co -Babbitt metalizing wire may be a patent-pending alloy the same as ASTM B-23 #3, however, Co has been added. This alloy incorporates a melting temperature of 240-422° C (464-792° F) and a hardness of 27-30 HV100. Co-Babbitt metalizing wire is usually used for terribly high hundreds that have multiple axes for stress-strain. It offers over doubly the tension-compression axial fatigue compared to Babbitt metalizing wire #2. Babbitt Metalizing Wire Manufacturer, Price in India We are a leading manufacturer of babbitt metalizing wire and provides at a low price in India. We export different sizes and different types of metalizing wire at a low price. We maintain the quality of the product and provide the best thermal spray results. We manufacture zinc spray gun, sand blasting machine, shot blasting machine, sand blasting hopper, thermal spray gun, arc spray gun, twin arc spray gun, metalizing gun, flame spray gun, zinc metalizing wire, zinc aluminium metalizing wire, nickel metalizing wire, copper metalizing wire, phosphorous bronze metalizing wire, tin metalizing wire and abrasive shots like copper slag, abrasive garnet, steel shots, cut wire shots also.