1 / 18

MHI#14 号機の2回目の EP2

MHI#14 号機の2回目の EP2. Period : 2011/2/8 ~ 2/14 Process : CP @flanges, EP2(20 μ m) under low current density, Improved 1 st Water Rinsing, Brushing @HOM & Flange using FM-20 , Degreasing(FM-20, 2%) [1hour] , Brushing @Flange, HPR x 2 [10 hours] , Assembly in C.R., Vacuum evacuation,

eve-alford
Download Presentation

MHI#14 号機の2回目の EP2

An Image/Link below is provided (as is) to download presentation Download Policy: Content on the Website is provided to you AS IS for your information and personal use and may not be sold / licensed / shared on other websites without getting consent from its author. Content is provided to you AS IS for your information and personal use only. Download presentation by click this link. While downloading, if for some reason you are not able to download a presentation, the publisher may have deleted the file from their server. During download, if you can't get a presentation, the file might be deleted by the publisher.

E N D

Presentation Transcript


  1. MHI#14号機の2回目のEP2 Period : 2011/2/8 ~2/14 Process : CP @flanges, EP2(20μm) under low current density, Improved 1st Water Rinsing, Brushing @HOM & Flange using FM-20, Degreasing(FM-20, 2%) [1hour], Brushing @Flange, HPR x 2 [10 hours], Assembly in C.R., Vacuum evacuation, Leak check, Baking @100℃ (48hours) Preparation : Washing vacuum components with ultrasonic, Cleaning in C.R. Workers : M. Sawabe, Kirk, M. Satoh (KEK), K. Nakamura, N. Tasaki, F. Tsukada (Assist Engineering Co.), T. Okada (K-VAC), S. Imada (Nihon Advanced Technology) Process log Status of working Monitor data during EP & Rinsing process Comparison of EP2 STF Cavity Group Meeting @2011/2/14 Kirk

  2. Condition of EP2 & Rinsing • EP acid (3/2のサンプルを使用) • Nb ingredient : 8.2g/ℓ • HF ingredient : 29 g/ℓ (全体38g/ℓの65%が反応に使われる) • Al ingredient : 15mg/ℓ • Current density : ~37mA/cm2 (最近の傾向より) • Cavity surface temperature : <35℃ • Control Voltage : 温度と電流密度を見ながら制御 • With normal N2 gas flow during extracting EP acid (8ℓ/min) • 1st water rinsing (1.5hours) • Improved version (25ℓ/minで20分間上下から流し続ける) • 1分毎に1秒間水抜きを繰り返す(40分間) • 最後の30分は10min (storing)/3min (flushing)で行う • Degreasing (1 hour) • FM-20(2%) • HPR (~10 hours) • 5h17m (6 turns, w/o blind flanges) • 4h25m (5 turns, w/ blind flanges) Brushing @HOM & Flange using FM-20 Brushing @Flange using FM-20 STF Cavity Group Meeting @2011/2/14

  3. Process log ① 2/8 10:00 CP @flanges 10:30~ Attachment of jigs for EP 11:41 Set cavity to EP bed with crane 12:00 Installation of cathode bar to cavity Lunch time 13:00 Set data logger to cavity (totally 12ch) Leak check with N2 gas [O.K.] 13:30 Meeting for tomorrow’s working procedure 13:50~ Vacuum parts rinsing with ultrasonic in C.R. 14:40 Guide for Iwate-Ken Giren @STF 16:30 HPR Trouble occurred! Not finished at top position by automatic operation 17:00 fin. STF Cavity Group Meeting @2011/2/14

  4. Process log ② 2/9 9:45 Cavity rotation starts / EP acid flow starts 9:56 EP2 starts 11:05 EP2 stops [1h09m00s] / Idling rotation (3 rpm / 20min) 11:10 Plastic case detachment 11:27 Idling rotation stops 11:29 EP acid is removed from cavity with N2 gas flow(0.020MPa) 11:42 First rinsing with ultra pure water starts 12:02 Flow rate of pure water is changed slightly due to low level 13:17 First rinsing with ultra pure water stops [1h30m] 13:24 Detachment of restriction jigs / Data logger detached 13:40 Un-installation of cathode bar from cavity / washing cathode bar 13:50 transferring cavity from EP bed to wagon / Checking inside cavity (No mark) 14:20 Detachment of jigs for EP / Detaching every blind flange / Checking inside cavity (No mark) [O.K.] 14:30 Brushing at every flange using FM-20 / Shower rinsing 14:40 Checking inside cavity (No mark) [O.K.] 14:42 Attachment of jigs for degreasing 14:47 Flowing FM-20 into cavity 14:54 Degreasing with ultrasonic starts 15:54 Degreasing with ultrasonic stops [1hour] 16:00 Removing FM-20 from cavity 16:05 Detachment of jigs for degreasing / Checking inside cavity (No mark) [O.K.] STF Cavity Group Meeting @2011/2/14

  5. Process log ③ 2/9 16:10 Brushing at every flange using FM-20 / Shower rinsing 16:28 Transferring cavity from wagon on turntable for HPR using crane 16:38 Checking tolerance between position of nozzle and center of beam pipe 16:39 1st HPR for inside cavity starts 21:56 1st HPR for inside cavity stops [5h17m] (6 turns) 22:05 Attaching only top flanges in C.R. 22:26 fin. 2/10 9:00 Attachment of blind flanges at bottom beam pipe for 2nd HPR 9:18 HPR outside cavity with blind flanges starts [15mins] 9:36 2nd HPR for inside cavity with blind flanges starts 14:00 2nd HPR for inside cavity with blind flanges stops [4h25m] (5 turns) 14:05 Cavity enters into C.R. 14:30 Assembly in C.R. (Class 10) starts(type of helicoflex is changed from In to Sn coating) 15:35 Assembly in C.R. (Class 10) finishes / Moving out from Class10 to Class1000 15:44 Vacuum evacuation starts with heat guns 16:00 Turbo pump status 100% (Normal operation, but abnormal noise) 16:20 Leak check thoroughly @~1.5x10-3Pa [O.K.] 16:35 Baking @100℃ starts 19:00 Cavity vacuum : 1.58 x 10-4Pa @108℃/105℃/88℃/44℃ (Cell#3/Cell#7/Top/Bottom) Max Vacuum Level just after baking start : ~1.5 x 10-3Pa STF Cavity Group Meeting @2011/2/14

  6. Process log ④ 2/12 16:45 Cavity vacuum : 1.23 x 10-5Pa @109℃/106℃/98℃/46℃ Ribbon heater at bottom beam pipe is broken! 16:50 Baking Off [48hours] / Ion Pump ON 17:15 Cavity vacuum : 1.43 x 10-6Pa @86℃/67℃/90℃/44℃ 2/14 8:52 Cavity vacuum : 1.01 x 10-7Pa / I.P head : 3.8 x 10-8Pa 9:25 MHI#14 goes out of clean room and moves to V.T.A. STF Cavity Group Meeting @2011/2/14

  7. Status of working ① 電極棒の先端(ビニルテープで保護されている) STF Cavity Group Meeting @2011/2/14

  8. Status of working ② EP後にブラシングをかける STF Cavity Group Meeting @2011/2/14

  9. Status of working ③ 前回のEP2時に9セルに見られた白い縞模様は無くなっていた STF Cavity Group Meeting @2011/2/14

  10. Status of 2nd EP2 for MHI#14 ① Tcavity voltage Treservoir current Troom Tcavity 平均電流密度が37mA/cm2程度になるように電圧を調整する。 (low current density EP) average current density STF Cavity Group Meeting @2011/2/14

  11. Status of 2nd EP2 for MHI#14 ② 左図は平均電流密度と電圧の相関 右図は定常状態での分布 target STF Cavity Group Meeting @2011/2/14

  12. 最近の定常状態の比較 今回は空洞内液温も電流密度もいずれも高かった。 ただし、電流の振れ幅はいつもよりは小さかった。 STF Cavity Group Meeting @2011/2/14

  13. Status of 2nd EP2 for MHI#14 ③ EP2の間の空洞表面温度の状況。 #1 #2 #3 #4 #5 #6 #7 #8 #9 #10 #11 #12 STF Cavity Group Meeting @2011/2/14

  14. Status of 2nd EP2 for MHI#14 ④ EP2の間の空洞表面温度の状況(前ページの最後の拡大図)。 #1 #2 #3 #4 #5 #6 #7 #8 #9 #10 #11 #12 STF Cavity Group Meeting @2011/2/14

  15. Status of UWR for MHI#14 ① 通信不良でデータが途中で何度か跳んでいる。 #1 #2 #3 #4 #5 #6 #7 #8 #9 #10 #11 #12 STF Cavity Group Meeting @2011/2/14

  16. Status of UWR for MHI#14 ② 一次洗浄中の空洞温度の状況(前ページの拡大図) #1 #2 #3 #4 #5 #6 #7 #8 #9 #10 #11 #12 STF Cavity Group Meeting @2011/2/14

  17. Status of UWR for MHI#14 ③ ① ①は最初の注水完了時。 ②は流量を増やした状態での洗浄中。 ③は流量を減らした状態での洗浄中。 ② ③ STF Cavity Group Meeting @2011/2/14

  18. Status of HPR for MHI#14 ノズルは1st HPRでは6往復、2nd HPRでも5往復させた。 2回目の方がTOCは下がったが、particleが逆に上がっている。 STF Cavity Group Meeting @2011/2/14