160 likes | 395 Views
Engineering Technology Division. Power Plant Construction and QA/QC Chapter 6 – Welding, Procedure and Operator Qualification. Chapter 6 – Welding, Procedure and Operator Qualification. Overview. All Pressure Vessel Welding Requires Welding Procedures
E N D
Engineering Technology Division Power Plant Construction and QA/QC Chapter 6 – Welding, Procedure and Operator Qualification
Chapter 6 – Welding, Procedure and Operator Qualification Overview • All Pressure Vessel Welding Requires Welding Procedures • All Pressure Vessel Welding Requires Welder Qualification • ASME Code Requires Procedure and Welder Qualification • Authorized Inspector Must Witness Procedure and Welder Quals • Authorized Inspector Must Witness a Sample of the Weld NDE
Chapter 6 – Welding, Procedure and Operator Qualification Welding Processes
Chapter 6 – Welding, Procedure and Operator Qualification Welding Basics • Welding is the process of joining two materials using an electric arc • Primary Welding Types • “Stick” – SMAW – Shielded Metal Arc Welding • “MIG” – GMAW – Gas Metal Arc Welding • “TIG” – GTAW – Gas Tungsten Arc Welding • “Sub Arc” – SAW – Submerged Arc Welding • Six Welding Positions – Flat, Horizontal, Vertical, Overhead, Horizontal Round and Inclined • Brazing and Soldering – Non Pressure Boundary
Chapter 6 – Welding, Procedure and Operator Qualification Welding Positions
Chapter 6 – Welding, Procedure and Operator Qualification SMAW Welding Basics • Flux Covered Rod • Negative Polarity • DC Voltage • Excellent Access • Wide Material Use
Chapter 6 – Welding, Procedure and Operator Qualification GMAW Welding Basics • Gas Cover • Positive Polarity • DC Voltage • Thin Materials • Wide Material Use • Fast Process
Chapter 6 – Welding, Procedure and Operator Qualification GTAW Welding Basics • Gas Cover • Negative Polarity • AC or DC Voltage • Wide Material Use • Manual Process
Chapter 6 – Welding, Procedure and Operator Qualification SAW Welding Basics • Powder Flux • Negative Polarity • DC Voltage • Thick Materials • Fast Deposition
Chapter 6 – Welding, Procedure and Operator Qualification Welding Procedure WPS – Welding Procedure Specifications PQR – Procedure Qualification Records WQ – Welder Qualification Records These items are based on a joint and material design by a Welding Engineer. NDE and bend testing (DE) is used to verify procedure compliance.
Chapter 6 – Welding, Procedure and Operator Qualification Welding Symbols
Chapter 6 – Welding, Procedure and Operator Qualification Welding Symbols
Chapter 6 – Welding, Procedure and Operator Qualification Welding Symbols
Chapter 6 – Welding, Procedure and Operator Qualification Destructive Testing Tensile Bend Charpy V Notch
Chapter 6 – Welding, Procedure and Operator Qualification Questions?